phezulu_emuva

Imikhiqizo

I-WFA White Aluminium oxide Powder


  • Umbala:Okumhlophe Okumsulwa
  • Isimo:I-Cubic ne-Angular ne-Sharp
  • I-Gravity ethize:≥ 3.95
  • Ukuqina kwe-Mohs:9.2 Mohs
  • Iphoyinti lokuncibilika:2150 ℃
  • Ukuminyana kwenqwaba:1.50-1.95g/cm3
  • I-Al2O3:99.4%Amaminithi
  • I-Na2O:0.30%Ubukhulu
  • Imininingwane Yomkhiqizo

    ISICELO

    Impushana ye-alumina ehlanganisiwe emhlophe yenziwe nge-high-purity low-sodium alumina powder ngokuncibilika ezingeni lokushisa eliphezulu, ukupholisa ikristalu, bese iyachoboza.I-aluminium ehlanganisiwe ye-aluminium oxide powder grit emhlophe ingaphansi kolawulo oluqinile ukuze kugcinwe ukusabalalisa kosayizi wokusanhlamvu nokubukeka okungaguquki.

    Ukusatshalaliswa kosayizi wokusanhlamvu kwempushana ye-alumina emhlophe ehlanganisiwe kuncane.Ngemuva kokucubungula, ukuhlanzeka okuphezulu okumhlophe kwe-corundum powder kunokusanhlamvu okugcwele, imiphetho ebukhali namakhona, ukusebenza kahle kokugaya okuphezulu, ukugqama kokupholisha okuphezulu.Ukusebenza kahle kokugaya kuphezulu kakhulu kunama-abrasive athambile njenge-silica.

    Ngenxa yokubukeka kahle, ubuso bento epholishiwe buba nesiphetho esiphakeme.Isetshenziswa kakhulu ekugayeni nasekupholishweni kwama-semiconductors, amakristalu, amabhodi esekethe, i-aluminium, insimbi, insimbi engagqwali, itshe, ingilazi, njll. Ikakhulukazi embonini yokugaya nokupholishwa kwensimbi engagqwali, i-aluminium, ithusi nezinye izinto zensimbi nemboni yengilazi. , ikhombisa ngokugcwele ukusebenza okuphezulu.

    I-Aluminiyamu Oksidi Yempushana Emhlophe

    I-White Fused Alumina Powder

    Okumhlophe, i-crystal α ngaphezu kuka-99%, ukuhlanzeka okuphezulu, ubulukhuni obuphezulu, nokuqina okuphezulu, amandla okusika aqinile, ukuqina kwamakhemikhali okuqinile, nokufakwa okuqinile.

    Ifomu le-Crystal isistimu ye-trigonal
    Ukuminyana kwangempela 3.90 g/cm3
    Ukuqina okuncane 2000 - 2200 Kg/mm2
    Mohs ubulukhuni 9

    Ukucaciswa Nokubunjwa Kwe-Alumina Ehlanganisiwe Emhlophe

    Ukucaciswa kosayizi we-particle kanye nokwakheka

    I-JIS

    240#,280#,320#,360#,400#,500#,600#,700#,800#,1000#,1200#,1500#,2000#,2500#,3000#,3500#,4000#,6000#,8000#,10000#,12500#

    Izinga laseYurophu

    F240,F280,F320,F360,F400,F500,F600,F800,F1000,F1200,F1500,F2000,F2500,F3000,F4000,F6000

    Izinga likazwelonke

    W63,W50,W40,W28,W20,W14,W10,W7,W5,W3.5,W2.5,W1.5,W1,W0.5

    Ukwakheka kwamakhemikhali

    Okusanhlamvu

    Ukwakheka kwamakhemikhali(%)

    I-Al2O3

    SiO2

    Fe2O3

    Na2O

    240#--3000#

    ≥99.50

    ≤0.10

    ≤0.03

    ≤0.22

    4000#-12500#

    ≥99.00

    ≤0.10

    ≤0.05

    ≤0.25

    01

    Awekho amathonya mayelana nombala wezingxenye ezicutshunguliwe.

    02

    Ingasetshenziswa ezinqubweni lapho insalela ye-iron powder ivinjelwe ngokuqinile.

    03

    Izinhlamvu zokubumba zifaneleka kakhulu ekusebenzeni kwe-sandblasting emanzi kanye nokupholisha.


  • Okwedlule:
  • Olandelayo:

  • 1.Ukuqhunyiswa kwesihlabathi, ukupholishwa nokugaya insimbi nengilazi.

    2.Ukugcwalisa upende, ukunamathela okungagugi, i-ceramic, ne-glaze.

    3.Ukwenziwa kwetshe lamafutha, itshe lokugaya, isondo lokugaya, i-sandpaper nendwangu ye-emery.

    I-4.Ukukhiqizwa kolwelwesi lwe-ceramic filter, amashubhu e-ceramic, amapuleti e-ceramic.

    5.Ukukhiqizwa koketshezi olucwebezelayo, i-wax eqinile kanye ne-wax ewuketshezi.

    6.Ngokusetshenziswa kwesitezi esingagugi.

    7.Ukugaya okuthuthukisiwe nokupholishwa kwamakristalu e-piezoelectric, ama-semiconductors, insimbi engagqwali, i-aluminium nezinye izinsimbi nezingezona izinsimbi.